When selecting carbon black grades, most ink engineers first focus on blackness, tinting strength and DBP oil absorption value. However, during actual production and trial runs, they frequently encounter problems such as unstable dispersion, system thickening, re-agglomeration during storage and abnormal curing, which cannot be resolved even with repeated grinding. At this point, two easily overlooked carbon black indicators should be prioritized for troubleshooting: volatile matter and pH value.

The volatile matter of carbon black mainly originates from oxygen-containing functional groups on the particle surface, including carboxyl groups, hydroxyl groups, quinone groups and so on. These groups directly determine the surface polarity of carbon black.

High-volatile-matter carbon black: Rich in surface oxygen-containing groups, it is more readily wetted by resins in water-based inks and polar solvent systems, featuring lower dispersion difficulty and better storage stability of ink slurry. Nevertheless, excessively high volatile matter increases the acidity of the system, and may interfere with photoinitiation in UV inks, slowing down the curing rate.

Low-volatile-matter carbon black: With fewer surface functional groups and stronger non-polarity, it is more suitable for non-polar solvent-based inks. Its drawback is poor wettability; stronger dispersants and higher grinding energy are required, and flocculation tends to occur.

The pH value of carbon black reflects the surface acidity and alkalinity of carbon black, and is inherently highly correlated with volatile matter. Most furnace pigment carbon blacks are weakly alkaline; carbon blacks subjected to oxidative post-treatment have a low pH and are classified as acidic carbon black. The pH value directly affects the overall acid-base balance of the ink system. If resins or additives are acid-base sensitive, pairing them with carbon black of greatly different pH values will disrupt the dispersion system. For instance, anionic dispersants will undergo charge neutralization when contacting strongly alkaline carbon black, causing abnormal viscosity rise of the ink and sedimentation after standing.

Here are several practical key points for grade selection in practice: For water-based flexographic and inkjet inks, carbon black with oxidative treatment, low pH and relatively high volatile matter is preferred to improve dispersion and color stability. For solvent-based gravure inks, carbon black with medium-to-low volatile matter and neutral to weakly alkaline properties can be selected to reduce side reactions in the system. When switching carbon black grades in an existing formula, blackness alone cannot be used for comparison. Volatile matter and pH must also be evaluated; otherwise batch-to-batch variation is very likely to occur. Note: Volatile matter is not equivalent to moisture. It is necessary to distinguish moisture tested at 105 °C from high-temperature volatiles tested at 950 °C, and the two test results should not be confused.

Many unexplained rheological anomalies in ink factories stem not from the grinding process, but from mismatching between the surface chemical properties of carbon black and the formulation system. Blackness is only an apparent property. Surface characteristic indicators such as volatile matter and pH are the fundamental keys to stable ink production and consistent printing performance.

www.eufuho.com

Comments

Popular posts from this blog

Printing knowledge - screen printing ink preparation and recycling method

Printing knowledge - field printing shows maximum saturation

Printing Knowledge - Printing Classification